EN 1652 Grade CuNi9Sn2 R450

Want to keep this datasheet? Save it now in your required format

Description

CuNi9Sn2 (CW351H) is comparable to CuNi9Sn2, mat. no. 2.0875, acc. to DIN 17664 : 1983-12. To the comparable DIN-mark applies: The material shows high strength specific values as well as favorable tarnish-proofness and a very good stress relaxation behaviour in spring-hard condition. CuNi9Sn2 has sufficient electrical and thermal conductivity. Favorable corrosion resistance in natural resp. industrial atmosphere. Also resistance to different waters, humidity, non-oxidizing acids, bases and saline solutions. No risk of stress corrosion. Processing properties: warm forming: good cold forming: very good machinability: unfavorable hard soldering: very good soft soldering: very good gas-shielded welding: very good burnishing: very good Application: For elastic components in relay, pushbutton switchers, connectors and receptacles in communications engineering, in EDP-systems, in consumer electronics equipment and in automobile electronics, for switcher components, soldering tags and frames, boxes for electrical components, carrier plates for integrated circuits an for conductor board pens. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.89 - 8.9 g/cm³

Show Material materials with Density of 8.89 - 8.9 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

140 GPa

Show Material materials with Elastic modulus of 140 GPa

Elongation A50

20.0 °C

4 - 6 %

Show Material materials with Elongation A50 of 4 - 6 %

Poisson's ratio

20.0 °C

0.34 [-]

Show Material materials with Poisson's ratio of 0.34 [-]

Tensile strength

20.0 °C

450 - 530 MPa

Show Material materials with Tensile strength of 450 - 530 MPa

Yield strength Rp0.2

20.0 °C

370 MPa

Show Material materials with Yield strength Rp0.2 of 370 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

1.55E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.55E-5 1/K

200.0 °C

1.59E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.59E-5 1/K

300.0 °C

1.66E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.66E-5 1/K

Melting point

915 - 1240 °C

Show Material materials with Melting point of 915 - 1240 °C

Typical for Wrought Copper Nickel Grade

Specific heat capacity

20.0 °C

370 J/(kg·K)

Show Material materials with Specific heat capacity of 370 J/(kg·K)

100.0 °C

390 J/(kg·K)

Show Material materials with Specific heat capacity of 390 J/(kg·K)

200.0 °C

410 J/(kg·K)

Show Material materials with Specific heat capacity of 410 J/(kg·K)

Unlock all property charts

Thermal conductivity

20.0 °C

48 W/(m·K)

Show Material materials with Thermal conductivity of 48 W/(m·K)

100.0 °C

56 W/(m·K)

Show Material materials with Thermal conductivity of 56 W/(m·K)

200.0 °C

65 W/(m·K)

Show Material materials with Thermal conductivity of 65 W/(m·K)

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

6.00E+6 - 6.40E+6 S/m

Show Material materials with Electrical conductivity of 6.00E+6 - 6.40E+6 S/m

Specific Electrical conductivity

10 - 11 % IACS

Show Material materials with Specific Electrical conductivity of 10 - 11 % IACS

Chemical properties

PropertyValue

Iron

0.3 %

Show Material materials with Iron of 0.3 %

Lead

0.03 %

Show Material materials with Lead of 0.03 %

Manganese

0.3 %

Show Material materials with Manganese of 0.3 %

Nickel

8.5 - 10.5 %

Show Material materials with Nickel of 8.5 - 10.5 %

Tin

1.8 - 2.8 %

Show Material materials with Tin of 1.8 - 2.8 %

Zinc

0.05 - 0.1 %

Show Material materials with Zinc of 0.05 - 0.1 %