EN 1652 Grade CuSn3Zn9 R380

Want to keep this datasheet? Save it now in your required format

Description

Material CuSn3Zn9, mat. No. CW454K, is predominantly used in electrical engineering. The multicomponent alloy is characterized by a considerably lower stress corrosion sensitivity compared to the copper-zinc-alloys. The spring properties come up to alloy CuSn4 (CW450K). For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.75 - 8.8 g/cm³

Show Material materials with Density of 8.75 - 8.8 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

126 GPa

Show Material materials with Elastic modulus of 126 GPa

Elongation

20.0 °C

22 %

Show Material materials with Elongation of 22 %

Elongation A50

20.0 °C

16 - 18 %

Show Material materials with Elongation A50 of 16 - 18 %

Poisson's ratio

20.0 °C

0.34 [-]

Show Material materials with Poisson's ratio of 0.34 [-]

Shear modulus

23.0 °C

40 GPa

Show Material materials with Shear modulus of 40 GPa

Typical for Wrought Copper Brass

Tensile strength

20.0 °C

380 - 430 MPa

Show Material materials with Tensile strength of 380 - 430 MPa

Yield strength Rp0.2

20.0 °C

200 MPa

Show Material materials with Yield strength Rp0.2 of 200 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

1.83E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.83E-5 1/K

300.0 °C

1.85E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.85E-5 1/K

Melting point

875 - 1075 °C

Show Material materials with Melting point of 875 - 1075 °C

Typical for Wrought Copper Brass

Specific heat capacity

20.0 °C

380 J/(kg·K)

Show Material materials with Specific heat capacity of 380 J/(kg·K)

200.0 °C

410 J/(kg·K)

Show Material materials with Specific heat capacity of 410 J/(kg·K)

Unlock all property charts

Thermal conductivity

20.0 °C

120 W/(m·K)

Show Material materials with Thermal conductivity of 120 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

1.60E+7 S/m

Show Material materials with Electrical conductivity of 1.60E+7 S/m

Specific Electrical conductivity

28 % IACS

Show Material materials with Specific Electrical conductivity of 28 % IACS

Chemical properties

PropertyValue

Iron

0.1 %

Show Material materials with Iron of 0.1 %

Lead

0.1 %

Show Material materials with Lead of 0.1 %

Nickel

0.2 %

Show Material materials with Nickel of 0.2 %

Phosphorus

0.2 %

Show Material materials with Phosphorus of 0.2 %

Tin

1.5 - 3.5 %

Show Material materials with Tin of 1.5 - 3.5 %

Zinc

7.5 - 10 %

Show Material materials with Zinc of 7.5 - 10 %