EN 1652 Grade CuAl8Fe3 R450

Want to keep this datasheet? Save it now in your required format

Description

CuAl8Fe3 (CW303G) is a wrought alloy of high strength, also at increased temperatures. The strength properties of cold formable wrought alloys are primarily dependent on the deformation grade. Tensile strength, yield strength and hardness rise according to the increasing cold forming grade. Elongation after fracture and contraction at fracture are decreasing. Thermal conductivity is reduced by the Al-content, electrical conductivity decreases according to the increasing AL-content. CuAl10Fe3Mn2 has a high strength at high temperatures up to approx. 300°C and a high endurance strength also at corrosion strain. The alloy is scaling resistant , shows a high wear resistance and a high corrosion resistance to saltwater, sulfite bases and mineral acids, it shows no erosion and cavitation sensitivity. Processing properties: warm forming: good cold forming: moderately machinability: good soft soldering: moderately hard soldering: moderately gas-shielded welding: good burnishing: good CuAl10Fe3Mn2 is used for plates for condenser and heat-transfer bottoms, for sheets in chemical apparatus engineering.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.7 g/cm³

Show Material materials with Density of 7.7 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

120 GPa

Show Material materials with Elastic modulus of 120 GPa

Elongation

20.0 °C

30 %

Show Material materials with Elongation of 30 %

Hardness, Vickers

20.0 °C

130 [-]

Show Material materials with Hardness, Vickers of 130 [-]

Poisson's ratio

23.0 °C

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Leaded Phosphor Bronze

Shear modulus

20.0 °C

45 GPa

Show Material materials with Shear modulus of 45 GPa

Tensile strength

20.0 °C

450 MPa

Show Material materials with Tensile strength of 450 MPa

Yield strength Rp0.2

20.0 °C

200 MPa

Show Material materials with Yield strength Rp0.2 of 200 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.5E-5 - 1.9E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.5E-5 - 1.9E-5 1/K

Typical for Leaded Phosphor Bronze

Specific heat capacity

23.0 °C

380 J/(kg·K)

Show Material materials with Specific heat capacity of 380 J/(kg·K)

Typical for Leaded Phosphor Bronze

Thermal conductivity

20.0 °C

65 W/(m·K)

Show Material materials with Thermal conductivity of 65 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

7.50E+6 S/m

Show Material materials with Electrical conductivity of 7.50E+6 S/m

Chemical properties

PropertyValue

Aluminium

6.5 - 8.5 %

Show Material materials with Aluminium of 6.5 - 8.5 %

Copper

84.95 %

Show Material materials with Copper of 84.95 %

Iron

1.5 - 3.5 %

Show Material materials with Iron of 1.5 - 3.5 %

Lead

0.05 %

Show Material materials with Lead of 0.05 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Nickel

1 %

Show Material materials with Nickel of 1 %

Silicon

0.2 %

Show Material materials with Silicon of 0.2 %

Tin

0.1 %

Show Material materials with Tin of 0.1 %

Zinc

0.5 %

Show Material materials with Zinc of 0.5 %