Description

Copper zinc (leaded brass) plates, sheet and circles for boilers, pressure vessels and hot water storage units.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.4 g/cm³

Show Material materials with Density of 8.4 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

-195.0 °C

108 GPa

Show Material materials with Elastic modulus of 108 GPa

-100.0 °C

106 GPa

Show Material materials with Elastic modulus of 106 GPa

20.0 °C

102 - 105 GPa

Show Material materials with Elastic modulus of 102 - 105 GPa

50.0 °C

100 GPa

Show Material materials with Elastic modulus of 100 GPa

100.0 °C

93 GPa

Show Material materials with Elastic modulus of 93 GPa

150.0 °C

91 GPa

Show Material materials with Elastic modulus of 91 GPa

200.0 °C

89 GPa

Show Material materials with Elastic modulus of 89 GPa

250.0 °C

83 GPa

Show Material materials with Elastic modulus of 83 GPa

Elongation

20.0 °C

30 %

Show Material materials with Elongation of 30 %

Hardness, Vickers

20.0 °C

80 [-]

Show Material materials with Hardness, Vickers of 80 [-]

Shear modulus

20.0 °C

37 GPa

Show Material materials with Shear modulus of 37 GPa

Tensile strength

20.0 °C

310 MPa

Show Material materials with Tensile strength of 310 MPa

Yield strength Rp0.2

20.0 °C

100 MPa

Show Material materials with Yield strength Rp0.2 of 100 MPa

Yield strength Rp1.0

50.0 °C

120 MPa

Show Material materials with Yield strength Rp1.0 of 120 MPa

100.0 °C

115 MPa

Show Material materials with Yield strength Rp1.0 of 115 MPa

150.0 °C

115 MPa

Show Material materials with Yield strength Rp1.0 of 115 MPa

200.0 °C

110 MPa

Show Material materials with Yield strength Rp1.0 of 110 MPa

Unlock all property charts

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

200.0 °C

2.04E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.04E-5 1/K

Melting point

875 - 1075 °C

Show Material materials with Melting point of 875 - 1075 °C

Typical for Wrought Copper Brass

Specific heat capacity

23.0 °C

371 - 418 J/(kg·K)

Show Material materials with Specific heat capacity of 371 - 418 J/(kg·K)

Typical for Wrought Copper Brass

Thermal conductivity

20.0 °C

109 W/(m·K)

Show Material materials with Thermal conductivity of 109 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

1.39E+7 S/m

Show Material materials with Electrical conductivity of 1.39E+7 S/m

Electrical resistivity

20.0 °C

7.2E-8 Ω·m

Show Material materials with Electrical resistivity of 7.2E-8 Ω·m

Chemical properties

PropertyValue

Aluminium

0.05 %

Show Material materials with Aluminium of 0.05 %

Copper

59 - 60.5 %

Show Material materials with Copper of 59 - 60.5 %

Iron

0.2 %

Show Material materials with Iron of 0.2 %

Lead

0.2 - 0.8 %

Show Material materials with Lead of 0.2 - 0.8 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %

Tin

0.2 %

Show Material materials with Tin of 0.2 %