Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.91 g/cm³

Show Material materials with Density of 8.91 g/cm³

Mechanical

PropertyTemperatureValue

Elongation

20.0 °C

8 - 10 %

Show Material materials with Elongation of 8 - 10 %

Elongation A100

20.0 °C

5 - 8 %

Show Material materials with Elongation A100 of 5 - 8 %

Hardness, Vickers

20.0 °C

165 - 200 [-]

Show Material materials with Hardness, Vickers of 165 - 200 [-]

Tensile strength

20.0 °C

440 - 570 MPa

Show Material materials with Tensile strength of 440 - 570 MPa

Yield strength Rp0.2

20.0 °C

400 - 440 MPa

Show Material materials with Yield strength Rp0.2 of 400 - 440 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

100.0 °C

1.63E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.63E-5 1/K

200.0 °C

1.7E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.7E-5 1/K

300.0 °C

1.76E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.76E-5 1/K

Chemical properties

PropertyValue

Chromium

0.5 - 1.2 %

Show Material materials with Chromium of 0.5 - 1.2 %

Iron

0.08 %

Show Material materials with Iron of 0.08 %

Silicon

0.1 %

Show Material materials with Silicon of 0.1 %

Zirconium

0.03 - 0.3 %

Show Material materials with Zirconium of 0.03 - 0.3 %