EN 12163 Grade CuZn28 M

Want to keep this datasheet? Save it now in your required format

Description

CuZn28 (CW504L) is an unhardenable wrought alloy. High hardness and strength parameter are achievable by cold forming only. Thermal and electrical conductivity are lower than for CuZn20. Corrosion resistance is similar to pure copper. Processing properties: warm forming: good cold forming: very good machinability: moderately hard and soft soldering: very good TIG-welding: good burnishing: good CuZn28 is used for deep drawing components and all types of sleeves, for automotive cooler, musical instruments, springing elements and clockfaces and as cladding material for ingot steel.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.55 - 8.6 g/cm³

Show Material materials with Density of 8.55 - 8.6 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

114 GPa

Show Material materials with Elastic modulus of 114 GPa

Shear modulus

20.0 °C

40 GPa

Show Material materials with Shear modulus of 40 GPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.7E-5 - 2.1E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.7E-5 - 2.1E-5 1/K

Typical for Wrought Copper Brass

Melting point

875 - 1075 °C

Show Material materials with Melting point of 875 - 1075 °C

Typical for Wrought Copper Brass

Specific heat capacity

20.0 °C

377 J/(kg·K)

Show Material materials with Specific heat capacity of 377 J/(kg·K)

Thermal conductivity

20.0 °C

130 W/(m·K)

Show Material materials with Thermal conductivity of 130 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

1.65E+7 S/m

Show Material materials with Electrical conductivity of 1.65E+7 S/m

Electrical resistivity

20.0 °C

6.1E-8 Ω·m

Show Material materials with Electrical resistivity of 6.1E-8 Ω·m

Chemical properties

PropertyValue

Aluminium

0.02 %

Show Material materials with Aluminium of 0.02 %

Copper

71 - 73 %

Show Material materials with Copper of 71 - 73 %

Iron

0.05 %

Show Material materials with Iron of 0.05 %

Lead

0.05 %

Show Material materials with Lead of 0.05 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %

Tin

0.1 %

Show Material materials with Tin of 0.1 %