EN 12163 Grade CuZn31Si1 M

Want to keep this datasheet? Save it now in your required format

Description

CuZn31Si1 (CW708R) is an unhardenable copper alloy. High hardness and strength parameter are achievable by cold forming only. Silicon decreases stress corrosion sensitivity. CuZn31Si1 shows favorable friction qualities. Processing properties: warm forming: moderately cold forming: good machinability: moderately hard soldering: moderately soft soldering: moderately TIG-welding: good burnishing: very good Appliction in machine, apparatus and plant construction particularly as friction elements such as bearing bushings, guidances etc.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.4 - 8.41 g/cm³

Show Material materials with Density of 8.4 - 8.41 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

108 GPa

Show Material materials with Elastic modulus of 108 GPa

Shear modulus

23.0 °C

40 GPa

Show Material materials with Shear modulus of 40 GPa

Typical for Wrought Copper Brass

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

200.0 °C

1.92E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.92E-5 1/K

Melting point

875 - 1075 °C

Show Material materials with Melting point of 875 - 1075 °C

Typical for Wrought Copper Brass

Specific heat capacity

20.0 °C

394 J/(kg·K)

Show Material materials with Specific heat capacity of 394 J/(kg·K)

100.0 °C

403 J/(kg·K)

Show Material materials with Specific heat capacity of 403 J/(kg·K)

200.0 °C

415 J/(kg·K)

Show Material materials with Specific heat capacity of 415 J/(kg·K)

Thermal conductivity

20.0 °C

71 W/(m·K)

Show Material materials with Thermal conductivity of 71 W/(m·K)

100.0 °C

79 W/(m·K)

Show Material materials with Thermal conductivity of 79 W/(m·K)

200.0 °C

86 W/(m·K)

Show Material materials with Thermal conductivity of 86 W/(m·K)

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

8.90E+6 S/m

Show Material materials with Electrical conductivity of 8.90E+6 S/m

Specific Electrical conductivity

15 % IACS

Show Material materials with Specific Electrical conductivity of 15 % IACS

Chemical properties

PropertyValue

Copper

66 - 70 %

Show Material materials with Copper of 66 - 70 %

Iron

0.4 %

Show Material materials with Iron of 0.4 %

Lead

0.8 %

Show Material materials with Lead of 0.8 %

Nickel

0.5 %

Show Material materials with Nickel of 0.5 %

Silicon

0.7 - 1.3 %

Show Material materials with Silicon of 0.7 - 1.3 %