EN 12163 Grade CuZn36Sn1Pb R400

Want to keep this datasheet? Save it now in your required format

Description

Material CuZn36Sn1Pb (CW712R) is incomparable to a DIN-make. It is used in the form of rods, hollow rods, profiles, wires, forging prematerial and forged parts.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.3 g/cm³

Show Material materials with Density of 8.3 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

100 - 125 GPa

Show Material materials with Elastic modulus of 100 - 125 GPa

Typical for Wrought Copper Brass

Elongation

20.0 °C

20 %

Show Material materials with Elongation of 20 %

Elongation A10

20.0 °C

13 - 16 %

Show Material materials with Elongation A10 of 13 - 16 %

Elongation A100

20.0 °C

10 %

Show Material materials with Elongation A100 of 10 %

Elongation A11.3

20.0 °C

16 %

Show Material materials with Elongation A11.3 of 16 %

Shear modulus

23.0 °C

40 GPa

Show Material materials with Shear modulus of 40 GPa

Typical for Wrought Copper Brass

Tensile strength

20.0 °C

400 MPa

Show Material materials with Tensile strength of 400 MPa

Yield strength Rp0.2

20.0 °C

200 - 210 MPa

Show Material materials with Yield strength Rp0.2 of 200 - 210 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.7E-5 - 2.1E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.7E-5 - 2.1E-5 1/K

Typical for Wrought Copper Brass

Melting point

875 - 1075 °C

Show Material materials with Melting point of 875 - 1075 °C

Typical for Wrought Copper Brass

Specific heat capacity

23.0 °C

371 - 418 J/(kg·K)

Show Material materials with Specific heat capacity of 371 - 418 J/(kg·K)

Typical for Wrought Copper Brass

Thermal conductivity

23.0 °C

100 - 234 W/(m·K)

Show Material materials with Thermal conductivity of 100 - 234 W/(m·K)

Typical for Wrought Copper Brass

Chemical properties

PropertyValue

Copper

61 - 63 %

Show Material materials with Copper of 61 - 63 %

Iron

0.1 %

Show Material materials with Iron of 0.1 %

Lead

0.2 - 0.6 %

Show Material materials with Lead of 0.2 - 0.6 %

Nickel

0.2 %

Show Material materials with Nickel of 0.2 %

Tin

1 - 1.5 %

Show Material materials with Tin of 1 - 1.5 %