EN 12163 Grade CuZn39Mn1AlPbSi M

Want to keep this datasheet? Save it now in your required format

Description

CuZn39Mn1AlPbSi (CW718R former identification: CuZn40Al1) is an unhardenable copper alloy. High hardness and strength values are achievable by cold forming only. Strength properties, corrosion resistance and oxidation resistance are increasable by Al-addition. CuZn39Mn1AlPbSi shows a mean wear resistance and favorable siding qualities. Processing properties: warm forming: very good cold forming: unfavorable machinability: moderately hard soldering: moderately soft soldering: unfavorable TIG-welding: moderately burnishing: very good The material is applicated for steering knuckle bushings, sliding bearings, sliding elements, worm gear rims and pinion gears.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.2 g/cm³

Show Material materials with Density of 8.2 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

106 GPa

Show Material materials with Elastic modulus of 106 GPa

Shear modulus

20.0 °C

40 GPa

Show Material materials with Shear modulus of 40 GPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

95.0 °C

2.16E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.16E-5 1/K

Melting point

875 - 1075 °C

Show Material materials with Melting point of 875 - 1075 °C

Typical for Wrought Copper Brass

Specific heat capacity

23.0 °C

371 - 418 J/(kg·K)

Show Material materials with Specific heat capacity of 371 - 418 J/(kg·K)

Typical for Wrought Copper Brass

Thermal conductivity

20.0 °C

71 W/(m·K)

Show Material materials with Thermal conductivity of 71 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

9.10E+6 S/m

Show Material materials with Electrical conductivity of 9.10E+6 S/m

Electrical resistivity

20.0 °C

1.1E-7 Ω·m

Show Material materials with Electrical resistivity of 1.1E-7 Ω·m

Chemical properties

PropertyValue

Aluminium

0.3 - 1.3 %

Show Material materials with Aluminium of 0.3 - 1.3 %

Copper

57 - 60 %

Show Material materials with Copper of 57 - 60 %

Iron

0.5 - 1 %

Show Material materials with Iron of 0.5 - 1 %

Lead

0.2 - 0.8 %

Show Material materials with Lead of 0.2 - 0.8 %

Manganese

0.8 - 1.8 %

Show Material materials with Manganese of 0.8 - 1.8 %

Nickel

0.5 - 1 %

Show Material materials with Nickel of 0.5 - 1 %

Silicon

0.2 - 0.8 %

Show Material materials with Silicon of 0.2 - 0.8 %

Tin

0.4 - 0.5 %

Show Material materials with Tin of 0.4 - 0.5 %