Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 7.6 g/cm³ Show Material materials with Density of 7.6 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 110 - 130 GPa Show Material materials with Elastic modulus of 110 - 130 GPa | Typical for Leaded Phosphor Bronze |
Hardness, Brinell | 20.0 °C | 130 - 170 [-] Show Material materials with Hardness, Brinell of 130 - 170 [-] | |
Hardness, Vickers | 20.0 °C | 135 - 175 [-] Show Material materials with Hardness, Vickers of 135 - 175 [-] | |
Poisson's ratio | 23.0 °C | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Specific heat capacity | 23.0 °C | 380 J/(kg·K) Show Material materials with Specific heat capacity of 380 J/(kg·K) | Typical for Leaded Phosphor Bronze |
Chemical properties
Property | Value |
---|---|
Aluminium | 9 - 10 % Show Material materials with Aluminium of 9 - 10 % |
Copper | 79.45 % Show Material materials with Copper of 79.45 % |
Iron | 0.5 - 1.5 % Show Material materials with Iron of 0.5 - 1.5 % |
Lead | 0.02 % Show Material materials with Lead of 0.02 % |
Manganese | 0.5 % Show Material materials with Manganese of 0.5 % |
Nickel | 1 % Show Material materials with Nickel of 1 % |
Silicon | 0.2 % Show Material materials with Silicon of 0.2 % |
Tin | 0.1 % Show Material materials with Tin of 0.1 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |
Do you have a technical question or need more information about this material?