Mechanical

PropertyTemperatureValue

Elongation

20.0 °C

20 %

Show Material materials with Elongation of 20 %

Elongation A10

20.0 °C

16 %

Show Material materials with Elongation A10 of 16 %

Tensile strength

20.0 °C

380 MPa

Show Material materials with Tensile strength of 380 MPa

Yield strength Rp0.2

20.0 °C

160 MPa

Show Material materials with Yield strength Rp0.2 of 160 MPa

Chemical properties

PropertyValue

Aluminium

0.05 %

Show Material materials with Aluminium of 0.05 %

Copper

59 - 60 %

Show Material materials with Copper of 59 - 60 %

Iron

0.2 %

Show Material materials with Iron of 0.2 %

Lead

0.8 - 1.6 %

Show Material materials with Lead of 0.8 - 1.6 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %

Tin

0.2 %

Show Material materials with Tin of 0.2 %