EN 12164 Grade CuZn39Pb1 R360

Want to keep this datasheet? Save it now in your required format

Description

CW611N is good to very good cold formable and machinable. Application: bending, riveting, embossing and upsetting parts

Related Standards

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.4 g/cm³

Show Material materials with Density of 8.4 g/cm³

Mechanical

PropertyTemperatureValue

Elongation

20.0 °C

20 - 25 %

Show Material materials with Elongation of 20 - 25 %

Elongation A100

20.0 °C

10 %

Show Material materials with Elongation A100 of 10 %

Elongation A11.3

20.0 °C

15 %

Show Material materials with Elongation A11.3 of 15 %

Tensile strength

20.0 °C

360 MPa

Show Material materials with Tensile strength of 360 MPa

Yield strength Rp0.2

20.0 °C

150 - 300 MPa

Show Material materials with Yield strength Rp0.2 of 150 - 300 MPa

Chemical properties

PropertyValue

Aluminium

0.05 %

Show Material materials with Aluminium of 0.05 %

Copper

59 - 60 %

Show Material materials with Copper of 59 - 60 %

Iron

0.2 %

Show Material materials with Iron of 0.2 %

Lead

0.8 - 1.6 %

Show Material materials with Lead of 0.8 - 1.6 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %

Tin

0.2 %

Show Material materials with Tin of 0.2 %