EN 12164 Grade CuSn4Pb4Zn4 R550

Want to keep this datasheet? Save it now in your required format

Description

Material CuSn4Pb4Zn4, mat. No. CW456K, is incomparable to a DIN-make. It is used in the form of bars.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.89 - 8.9 g/cm³

Show Material materials with Density of 8.89 - 8.9 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

103 GPa

Show Material materials with Elastic modulus of 103 GPa

Elongation A10

20.0 °C

5 %

Show Material materials with Elongation A10 of 5 %

Elongation A100

20.0 °C

3 %

Show Material materials with Elongation A100 of 3 %

Elongation A11.3

20.0 °C

11 %

Show Material materials with Elongation A11.3 of 11 %

Poisson's ratio

23.0 °C

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Leaded Phosphor Bronze

Tensile strength

20.0 °C

550 MPa

Show Material materials with Tensile strength of 550 MPa

Yield strength Rp0.2

20.0 °C

480 - 500 MPa

Show Material materials with Yield strength Rp0.2 of 480 - 500 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

100.0 °C

1.63E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.63E-5 1/K

300.0 °C

1.73E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.73E-5 1/K

Specific heat capacity

20.0 °C

380 J/(kg·K)

Show Material materials with Specific heat capacity of 380 J/(kg·K)

200.0 °C

410 J/(kg·K)

Show Material materials with Specific heat capacity of 410 J/(kg·K)

Unlock all property charts

Thermal conductivity

20.0 °C

86.5 - 87 W/(m·K)

Show Material materials with Thermal conductivity of 86.5 - 87 W/(m·K)

200.0 °C

109 W/(m·K)

Show Material materials with Thermal conductivity of 109 W/(m·K)

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

1.20E+7 S/m

Show Material materials with Electrical conductivity of 1.20E+7 S/m

Specific Electrical conductivity

21 % IACS

Show Material materials with Specific Electrical conductivity of 21 % IACS

Chemical properties

PropertyValue

Iron

0.1 %

Show Material materials with Iron of 0.1 %

Lead

3.5 - 4.5 %

Show Material materials with Lead of 3.5 - 4.5 %

Nickel

0.2 %

Show Material materials with Nickel of 0.2 %

Phosphorus

0.01 - 0.4 %

Show Material materials with Phosphorus of 0.01 - 0.4 %

Tellurium

0.2 %

Show Material materials with Tellurium of 0.2 %

Tin

3.5 - 4.5 %

Show Material materials with Tin of 3.5 - 4.5 %

Zinc

3.5 - 4.5 %

Show Material materials with Zinc of 3.5 - 4.5 %