Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 100 - 125 GPa Show Material materials with Elastic modulus of 100 - 125 GPa | Typical for Wrought Copper Brass |
Hardness, Rockwell B | 23.0 °C | 87 - 92 [-] Show Material materials with Hardness, Rockwell B of 87 - 92 [-] | |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 75 - 78 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 75 - 78 [-] | |
Shear modulus | 23.0 °C | 40 GPa Show Material materials with Shear modulus of 40 GPa | Typical for Wrought Copper Brass |
Tensile strength | 23.0 °C | 595 - 655 MPa Show Material materials with Tensile strength of 595 - 655 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Melting point | 875 - 1075 °C Show Material materials with Melting point of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Specific heat capacity | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Specific heat capacity of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Thermal conductivity | 23.0 °C | 100 - 234 W/(m·K) Show Material materials with Thermal conductivity of 100 - 234 W/(m·K) | Typical for Wrought Copper Brass |
Chemical properties
Property | Value |
---|---|
Copper | 62 - 65 % Show Material materials with Copper of 62 - 65 % |
Iron | 0.1 % Show Material materials with Iron of 0.1 % |
Lead | 0.25 - 0.7 % Show Material materials with Lead of 0.25 - 0.7 % |