EN 12167 Grade CuCo2Be H230

Want to keep this datasheet? Save it now in your required format

Description

Cuco2Be, mat. No CW104C, is counted among hardenable, low alloyed copper alloys. To the comparable make Cuco2Be, mat. No 2.1285, acc. to DIN 17666 : 1983-12 applies: CuCo2Be achieves compared to CuBe2 at slightly lower hardness and strength values higher electrical and thermal conductivity. The temperature for removal of workhardening approximates 500°C, high corrosion resistance. Processing properties: hot and cold forming: good machinability: moderately hard and soft soldering: good gas shielded welding: good burnishing: good Application: In relay and switch construction for high loadable, live springs and for radiant heaters at semi conductors. Furthermore for resistance and welding electrodes as well as for pistons, plunger and punching tools. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.8 - 8.9 g/cm³

Show Material materials with Density of 8.8 - 8.9 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

138 GPa

Show Material materials with Elastic modulus of 138 GPa

Hardness, Brinell

20.0 °C

230 - 310 [-]

Show Material materials with Hardness, Brinell of 230 - 310 [-]

Hardness, Vickers

20.0 °C

230 - 290 [-]

Show Material materials with Hardness, Vickers of 230 - 290 [-]

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

300.0 °C

1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K

Max service temperature, long

0 - 350 °C

Show Material materials with Max service temperature, long of 0 - 350 °C

Melting point

855 - 1090 °C

Show Material materials with Melting point of 855 - 1090 °C

Typical for Wrought Copper High Copper Alloy

Specific heat capacity

23.0 °C

360 - 420 J/(kg·K)

Show Material materials with Specific heat capacity of 360 - 420 J/(kg·K)

Typical for Wrought Copper High Copper Alloy

Thermal conductivity

20.0 °C

192 - 239 W/(m·K)

Show Material materials with Thermal conductivity of 192 - 239 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

2.50E+7 - 3.20E+7 S/m

Show Material materials with Electrical conductivity of 2.50E+7 - 3.20E+7 S/m

Specific Electrical conductivity

43 % IACS

Show Material materials with Specific Electrical conductivity of 43 % IACS

Chemical properties

PropertyValue

Beryllium

0.4 - 0.7 %

Show Material materials with Beryllium of 0.4 - 0.7 %

Cobalt

2 - 2.8 %

Show Material materials with Cobalt of 2 - 2.8 %

Iron

0.2 %

Show Material materials with Iron of 0.2 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %