General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 8.9 - 8.92 g/cm³ Show Material materials with Density of 8.9 - 8.92 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 20.0 °C | 130 GPa Show Material materials with Elastic modulus of 130 GPa |
Hardness, Brinell | 20.0 °C | 120 - 160 [-] Show Material materials with Hardness, Brinell of 120 - 160 [-] |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.63E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.63E-5 1/K | |
200.0 °C | 1.7E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.7E-5 1/K | ||
300.0 °C | 1.76E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.76E-5 1/K | ||
Melting point | 855 - 1090 °C Show Material materials with Melting point of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Specific heat capacity | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Specific heat capacity of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Thermal conductivity | 20.0 °C | 320 W/(m·K) Show Material materials with Thermal conductivity of 320 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 20.0 °C | 4.30E+7 - 4.60E+7 S/m Show Material materials with Electrical conductivity of 4.30E+7 - 4.60E+7 S/m |
Specific Electrical conductivity | 74 - 79 % IACS Show Material materials with Specific Electrical conductivity of 74 - 79 % IACS |
Chemical properties
Property | Value |
---|---|
Chromium | 0.5 - 1.2 % Show Material materials with Chromium of 0.5 - 1.2 % |
Iron | 0.08 % Show Material materials with Iron of 0.08 % |
Silicon | 0.1 % Show Material materials with Silicon of 0.1 % |