The material according this standard is used for seamless, round tubes for heat exchangers, condensers, evaporators and desalination equipment. It can be used for the working in sea water.

Related Standards

Equivalent Materials

This material data has been provided by WIAM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.9 g/cm³

Show Material materials with Density of 8.9 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

156 GPa

Show Material materials with Elastic modulus of 156 GPa

Elongation

20.0 °C

30 %

Show Material materials with Elongation of 30 %

Tensile strength

20.0 °C

420 MPa

Show Material materials with Tensile strength of 420 MPa

Yield strength Rp0.2

20.0 °C

150 MPa

Show Material materials with Yield strength Rp0.2 of 150 MPa

50.0 °C

150 MPa

Show Material materials with Yield strength Rp0.2 of 150 MPa

100.0 °C

140 MPa

Show Material materials with Yield strength Rp0.2 of 140 MPa

150.0 °C

135 MPa

Show Material materials with Yield strength Rp0.2 of 135 MPa

200.0 °C

125 MPa

Show Material materials with Yield strength Rp0.2 of 125 MPa

250.0 °C

120 MPa

Show Material materials with Yield strength Rp0.2 of 120 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.4E-5 - 1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.4E-5 - 1.8E-5 1/K

Typical for Wrought Copper Nickel Grade

Melting point

915 - 1240 °C

Show Material materials with Melting point of 915 - 1240 °C

Typical for Wrought Copper Nickel Grade

Specific heat capacity

23.0 °C

375 - 398 J/(kg·K)

Show Material materials with Specific heat capacity of 375 - 398 J/(kg·K)

Typical for Wrought Copper Nickel Grade

Thermal conductivity

23.0 °C

21 - 195 W/(m·K)

Show Material materials with Thermal conductivity of 21 - 195 W/(m·K)

Typical for Wrought Copper Nickel Grade

Chemical properties

PropertyValue

Carbon

0.05 %

Show Material materials with Carbon of 0.05 %

Cobalt

0.1 %

Show Material materials with Cobalt of 0.1 %

Iron

1.5 - 2.5 %

Show Material materials with Iron of 1.5 - 2.5 %

Lead

0.02 %

Show Material materials with Lead of 0.02 %

Manganese

1.5 - 2.5 %

Show Material materials with Manganese of 1.5 - 2.5 %

Nickel

29 - 32 %

Show Material materials with Nickel of 29 - 32 %

Phosphorus

0.02 %

Show Material materials with Phosphorus of 0.02 %

Sulfur

0.05 %

Show Material materials with Sulfur of 0.05 %

Tin

0.05 %

Show Material materials with Tin of 0.05 %

Zinc

0.5 %