UNS C11300 O25

Want to keep this datasheet? Save it now in your required format

Description

Equivalent Materials

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

9 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

120 GPa at 23 °C

Show Wrought Copper Pure / Low Alloyed Copper materials with Elastic modulus of 120 GPa at 23 °C

Poisson's ratio

ν

0.34 [-] at 23 °C

Show Wrought Copper Pure / Low Alloyed Copper materials with Poisson's ratio of 0.34 [-] at 23 °C

Typical for Wrought Copper Pure / Low Alloyed Copper

Shear modulus

G

48 GPa at 23 °C

Show Wrought Copper Pure / Low Alloyed Copper materials with Shear modulus of 48 GPa at 23 °C

Typical for Wrought Copper Pure / Low Alloyed Copper

Tensile strength

Rm

230 MPa at 23 °C

Show Wrought Copper Pure / Low Alloyed Copper materials with Tensile strength of 230 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

1.6E-5 1/K at 23 °C

Melting point

Tm

965 - 1100 °C

Typical for Wrought Copper Pure / Low Alloyed Copper

Specific heat capacity

cp

390 J/(kg·K) at 23 °C

Thermal conductivity

λ

390 W/(m·K) at 23 °C

Chemical properties

Element

Weight %

Comment

Cu

99.85 - 99.97 %

Ag

0.03 - 0.05 %

Other

0 - 0.1 %

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.