UNS C63000 O25

Want to keep this datasheet? Save it now in your required format

Description

Equivalent Materials

Ashby charts

See where UNS C63000 O25 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

8.3 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

120 GPa at 23 °C

Show Wrought Copper Bronze Aluminium Bronze materials with Elastic modulus of 120 GPa at 23 °C

Elongation

A

12 % at 23 °C

Show Wrought Copper Bronze Aluminium Bronze materials with Elongation of 12 % at 23 °C

Poisson's ratio

ν

0.33 [-] at 23 °C

Show Wrought Copper Bronze Aluminium Bronze materials with Poisson's ratio of 0.33 [-] at 23 °C

Typical for Leaded Phosphor Bronze

Tensile strength

Rm

670 MPa at 23 °C

Show Wrought Copper Bronze Aluminium Bronze materials with Tensile strength of 670 MPa at 23 °C

Yield strength

YS

340 MPa at 23 °C

Show Wrought Copper Bronze Aluminium Bronze materials with Yield strength of 340 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

1.7E-5 1/K at 23 °C

Melting point

Tm

1040 °C

Specific heat capacity

cp

440 J/(kg·K) at 23 °C

Thermal conductivity

λ

39 W/(m·K) at 23 °C

Chemical properties

Element

Weight %

Comment

Cu

76.8 - 85 %

Al

9 - 11 %

Ni

4 - 5.5 %

Fe

2 - 4 %

Mn

0 - 1.5 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.