UNS C63000 O32

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperature

Density

8.3 g/cm³

Show Material materials with Density of 8.3 g/cm³ at 23.0 °C

23.0 °C

Mechanical

PropertyValueTemperatureComment

Elastic modulus

120 GPa

Show Material materials with Elastic modulus of 120 GPa at 23.0 °C

23.0 °C

Elongation

12 %

Show Material materials with Elongation of 12 % at 23.0 °C

23.0 °C

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-] at 23.0 °C

23.0 °C

Typical for Leaded Phosphor Bronze

Tensile strength

790 MPa

Show Material materials with Tensile strength of 790 MPa at 23.0 °C

23.0 °C

Yield strength

400 MPa

Show Material materials with Yield strength of 400 MPa at 23.0 °C

23.0 °C

Thermal

PropertyValueTemperature

Coefficient of thermal expansion

1.7E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.7E-5 1/K at 23.0 °C

23.0 °C

Melting point

1040 °C

Show Material materials with Melting point of 1040 °C

Specific heat capacity

440 J/(kg·K)

Show Material materials with Specific heat capacity of 440 J/(kg·K) at 23.0 °C

23.0 °C

Thermal conductivity

39 W/(m·K)

Show Material materials with Thermal conductivity of 39 W/(m·K) at 23.0 °C

23.0 °C

Chemical properties

Property

Aluminium

9 - 11 %

Copper

76.8 - 85 %

Iron

2 - 4 %

Manganese

0 - 1.5 %

Nickel

4 - 5.5 %

Other

0 - 0.5 %

Silicon

0 - 0.25 %

Tin

0 - 0.2 %

Zinc

0 - 0.3 %