Density
ρ8.9 g/cm³ at 23 °C
Coefficient of thermal expansion
α1.6E-5 1/K at 23 °C
Melting point
Tm1080 °C
Specific heat capacity
cp390 J/(kg·K) at 23 °C
Thermal conductivity
λ260 W/(m·K) at 23 °C
Element
Weight %
Comment
96.8 - 97.8 %
2.1 - 2.6 %
0.05 - 0.2 %
0.02 - 0.15 %
0 - 0.03 %
This material data has been provided by MakeItFrom.com.