Density

ρ

8.8 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

120 GPa at 23 °C

Show Wrought Copper Bronze Silicon Bronze materials with Elastic modulus of 120 GPa at 23 °C

Elongation

A

50 % at 23 °C

Show Wrought Copper Bronze Silicon Bronze materials with Elongation of 50 % at 23 °C

Poisson's ratio

ν

0.33 [-] at 23 °C

Show Wrought Copper Bronze Silicon Bronze materials with Poisson's ratio of 0.33 [-] at 23 °C

Typical for Leaded Phosphor Bronze

Tensile strength

Rm

280 MPa at 23 °C

Show Wrought Copper Bronze Silicon Bronze materials with Tensile strength of 280 MPa at 23 °C

Yield strength

YS

110 MPa at 23 °C

Show Wrought Copper Bronze Silicon Bronze materials with Yield strength of 110 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

1.8E-5 1/K at 23 °C

Melting point

Tm

1030 °C

Specific heat capacity

cp

380 J/(kg·K) at 23 °C

Thermal conductivity

λ

57 W/(m·K) at 23 °C

Chemical properties

Element

Weight %

Comment

Cu

94.5 - 99.2 %

Si

0.8 - 2 %

Fe

0 - 0.8 %

Pb

0 - 0.05 %

Mn

0 - 0.7 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.