UNS C10100 OS050

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperature

Density

9 g/cm³

Show Material materials with Density of 9 g/cm³ at 23.0 °C

23.0 °C

Mechanical

PropertyValueTemperatureComment

Elastic modulus

120 GPa

Show Material materials with Elastic modulus of 120 GPa at 23.0 °C

23.0 °C

Elongation

50 %

Show Material materials with Elongation of 50 % at 23.0 °C

23.0 °C

Poisson's ratio

0.34 [-]

Show Material materials with Poisson's ratio of 0.34 [-] at 23.0 °C

23.0 °C

Typical for Wrought Copper Pure / Low Alloyed Copper

Shear modulus

48 GPa

Show Material materials with Shear modulus of 48 GPa at 23.0 °C

23.0 °C

Typical for Wrought Copper Pure / Low Alloyed Copper

Tensile strength

220 MPa

Show Material materials with Tensile strength of 220 MPa at 23.0 °C

23.0 °C

Yield strength

69 MPa

Show Material materials with Yield strength of 69 MPa at 23.0 °C

23.0 °C

Thermal

PropertyValueTemperature

Coefficient of thermal expansion

1.7E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.7E-5 1/K at 23.0 °C

23.0 °C

Melting point

1080 °C

Show Material materials with Melting point of 1080 °C

Specific heat capacity

390 J/(kg·K)

Show Material materials with Specific heat capacity of 390 J/(kg·K) at 23.0 °C

23.0 °C

Thermal conductivity

390 W/(m·K)

Show Material materials with Thermal conductivity of 390 W/(m·K) at 23.0 °C

23.0 °C

Chemical properties

Property

Copper

99.99 - 100 %

Lead

0 - 1E-3 %

Oxygen

0 - 5E-4 %

Phosphorus

0 - 3E-4 %

Zinc

0 - 1E-4 %