This website uses cookies to improve service quality. You will find more information about cookies on the privacy policy page.
Specific Electrical conductivity
5.80E+8 % IACS
Density ρ
9 g/cm³ at 20 °C
Elastic modulus E
120 GPa at 20 °C
Elongation A
50 % at 20 °C
Tensile strength Rm
220 MPa at 20 °C
Yield strength YS
69 MPa at 20 °C
Coefficient of thermal expansion α
1.7E-5 1/K at 20 °C
Melting point Tm
1070 °C
Specific heat capacity cp
390 J/(kg·K) at 20 °C
Thermal conductivity λ
390 W/(m·K) at 20 °C
Element
Weight %
Comment
99.9 - 100 %
0 - 0.1 %
This material data has been provided by MakeItFrom.com.