General
Property | Value | Temperature |
---|---|---|
Density | 8.41 - 8.8 g/cm³ Show Material materials with Density of 8.41 - 8.8 g/cm³ at 23.0 °C | 23.0 °C |
Dimension
Property | Value | Comment |
---|---|---|
Diameter | 0.76 - 76 mm Show Material materials with Diameter of 0.76 - 76 mm | |
Length | 610 - 91000 mm Show Material materials with Length of 610 - 91000 mm | max. |
Outside diameter | 9.5 - 76 mm Show Material materials with Outside diameter of 9.5 - 76 mm | |
Thickness | 4.8 - 76 mm Show Material materials with Thickness of 4.8 - 76 mm | |
Width | 305 - 559 mm Show Material materials with Width of 305 - 559 mm |
Mechanical
Property | Value | Temperature |
---|---|---|
Elastic modulus | 120 - 131 GPa Show Material materials with Elastic modulus of 120 - 131 GPa at 23.0 °C | 23.0 °C |
Elongation | 2 - 32 % Show Material materials with Elongation of 2 - 32 % at 23.0 °C | 23.0 °C |
Tensile strength | 490 - 1450 MPa Show Material materials with Tensile strength of 490 - 1450 MPa at 23.0 °C | 23.0 °C |
Yield strength | 160 MPa Show Material materials with Yield strength of 160 MPa at 23.0 °C | 23.0 °C |
Yield strength Rp0.2 | 860 - 1280 MPa Show Material materials with Yield strength Rp0.2 of 860 - 1280 MPa at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature |
---|---|---|
Coefficient of thermal expansion | 1.6E-5 - 1.75E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 1.75E-5 1/K at 23.0 °C | 23.0 °C |
Melting point | 870 °C Show Material materials with Melting point of 870 °C | |
Specific heat capacity | 410 J/(kg·K) Show Material materials with Specific heat capacity of 410 J/(kg·K) at 23.0 °C | 23.0 °C |
Thermal conductivity | 105 - 110 W/(m·K) Show Material materials with Thermal conductivity of 105 - 110 W/(m·K) at 23.0 °C | 23.0 °C |
Electrical
Property | Value | Temperature |
---|---|---|
Electrical resistivity | 5.8E-6 - 6.9E-6 Ω·m Show Material materials with Electrical resistivity of 5.8E-6 - 6.9E-6 Ω·m at 23.0 °C | 23.0 °C |
Specific Electrical conductivity | 25 - 30 % IACS Show Material materials with Specific Electrical conductivity of 25 - 30 % IACS |
Magnetic
Property | Value | Temperature | Comment |
---|---|---|---|
Relative magnetic permeability | 1 [-] Show Material materials with Relative magnetic permeability of 1 [-] at 23.0 °C | 23.0 °C | max. |
Chemical properties
Property | ||
---|---|---|
Aluminium | 0 - 0.2 % | |
Beryllium | 1.6 - 1.85 % | |
Cobalt | 0.2 % | min. Nickel + Cobalt |
Copper | 96.3 - 98.2 % | Balance |
Iron | 0 - 0.6 % | max., Nickel + Cobalt + Iron |
Nickel | 0.2 - 0.6 % | min. Nickel + Cobalt |
Other | 0 - 0.5 % | |
Silicon | 0 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include wear plates and resistance welding components.,Typical applications include bushings, bearings and resistance welding components.,Alloy 165 tube is used in crucial telecommunications applications including undersea instrument housings and repeater housings. |