General
Property | Value | Temperature |
---|---|---|
Density | 8.9 g/cm³ Show Material materials with Density of 8.9 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature |
---|---|---|
Elastic modulus | 130 GPa Show Material materials with Elastic modulus of 130 GPa at 23.0 °C | 23.0 °C |
Elongation | 11 % Show Material materials with Elongation of 11 % at 23.0 °C | 23.0 °C |
Tensile strength | 400 MPa Show Material materials with Tensile strength of 400 MPa at 23.0 °C | 23.0 °C |
Yield strength | 390 MPa Show Material materials with Yield strength of 390 MPa at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature |
---|---|---|
Coefficient of thermal expansion | 1.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K at 23.0 °C | 23.0 °C |
Melting point | 1070 °C Show Material materials with Melting point of 1070 °C | |
Specific heat capacity | 390 J/(kg·K) Show Material materials with Specific heat capacity of 390 J/(kg·K) at 23.0 °C | 23.0 °C |
Thermal conductivity | 320 W/(m·K) Show Material materials with Thermal conductivity of 320 W/(m·K) at 23.0 °C | 23.0 °C |
Chemical properties
Property | ||
---|---|---|
Chromium | 0.6 - 1.2 % | |
Copper | 98.6 - 99.4 % | |
Iron | 0 - 0.1 % | |
Lead | 0 - 0.05 % | |
Silicon | 0 - 0.1 % |