General
Property | Value | Temperature |
---|---|---|
Density | 8.9 g/cm³ Show Material materials with Density of 8.9 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Thermal
Property | Value | Temperature |
---|---|---|
Coefficient of thermal expansion | 1.6E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.6E-5 1/K at 23.0 °C | 23.0 °C |
Melting point | 1030 °C Show Material materials with Melting point of 1030 °C | |
Specific heat capacity | 390 J/(kg·K) Show Material materials with Specific heat capacity of 390 J/(kg·K) at 23.0 °C | 23.0 °C |
Thermal conductivity | 220 W/(m·K) Show Material materials with Thermal conductivity of 220 W/(m·K) at 23.0 °C | 23.0 °C |
Chemical properties
Property | ||
---|---|---|
Aluminium | 0 - 0.2 % | |
Beryllium | 0.15 - 0.5 % | |
Copper | 95.7 - 98.7 % | |
Iron | 0 - 0.2 % | |
Lead | 0.2 - 0.6 % | |
Nickel | 1 - 1.4 % | |
Other | 0 - 0.5 % | |
Silicon | 0 - 0.2 % | |
Tin | 0 - 0.25 % | |
Zirconium | 0 - 0.5 % |