General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.8 g/cm³ Show Material materials with Density of 8.8 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 120 GPa Show Material materials with Elastic modulus of 120 GPa |
Elongation | 23.0 °C | 1.2 % Show Material materials with Elongation of 1.2 % |
Tensile strength | 23.0 °C | 1280 MPa Show Material materials with Tensile strength of 1280 MPa |
Yield strength | 23.0 °C | 1150 MPa Show Material materials with Yield strength of 1150 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.6E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.6E-5 1/K |
Melting point | 870 °C Show Material materials with Melting point of 870 °C | |
Specific heat capacity | 23.0 °C | 410 J/(kg·K) Show Material materials with Specific heat capacity of 410 J/(kg·K) |
Thermal conductivity | 23.0 °C | 110 W/(m·K) Show Material materials with Thermal conductivity of 110 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 0 - 0.2 % Show Material materials with Aluminium of 0 - 0.2 % |
Beryllium | 1.6 - 1.8 % Show Material materials with Beryllium of 1.6 - 1.8 % |
Copper | 96.3 - 98.2 % Show Material materials with Copper of 96.3 - 98.2 % |
Iron | 0 - 0.4 % Show Material materials with Iron of 0 - 0.4 % |
Nickel | 0.2 - 0.6 % Show Material materials with Nickel of 0.2 - 0.6 % |
Other | 0 - 0.5 % Show Material materials with Other of 0 - 0.5 % |
Silicon | 0 - 0.2 % Show Material materials with Silicon of 0 - 0.2 % |