This website uses cookies to improve service quality. You will find more information about cookies on the privacy policy page.
Specific Electrical conductivity
2.32E+8 % IACS
Density ρ
8.9 g/cm³ at 20 °C
Elastic modulus E
120 GPa at 20 °C
Tensile strength Rm
670 MPa at 20 °C
Coefficient of thermal expansion α
1.6E-5 1/K at 20 °C
Melting point Tm
1080 °C
Specific heat capacity cp
390 J/(kg·K) at 20 °C
Thermal conductivity λ
170 W/(m·K) at 20 °C
Element
Weight %
Comment
92.7 - 97.5 %
2.2 - 4.2 %
0.25 - 1.2 %
0.05 - 0.3 %
0 - 0.05 %
This material data has been provided by MakeItFrom.com.