ASTM B197 Grade C17200 TM04

Alternative and trade names
Alloy 25 (C17200) Wire
Want to keep this datasheet? Save it now in your required format

Description

Materion Performance Alloys’ Alloy 25 wire provides the highest strength of any copper alloy, with electrical conductivity considerably greater than other high strength copper alloys. This alloy features good stress relaxation resistance and high fatigue strength.

Related Standards

Equivalent Materials

This material data has been provided by MakeItFrom.com,Materion Brush GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperature

Density

8.36 - 8.8 g/cm³

Show Material materials with Density of 8.36 - 8.8 g/cm³ at 23.0 °C

23.0 °C

Dimension

PropertyValue

Diameter

1.27 - 12.7 mm

Show Material materials with Diameter of 1.27 - 12.7 mm

Mechanical

PropertyValueTemperature

Elastic modulus

130 - 131 GPa

Show Material materials with Elastic modulus of 130 - 131 GPa at 23.0 °C

23.0 °C

Elongation

10 - 75 %

Show Material materials with Elongation of 10 - 75 % at 23.0 °C

23.0 °C

Tensile strength

410 - 980 MPa

Show Material materials with Tensile strength of 410 - 980 MPa at 23.0 °C

23.0 °C

Yield strength

850 MPa

Show Material materials with Yield strength of 850 MPa at 23.0 °C

23.0 °C

Yield strength Rp0.2

130 - 210 MPa

Show Material materials with Yield strength Rp0.2 of 130 - 210 MPa at 23.0 °C

23.0 °C

Thermal

PropertyValueTemperature

Coefficient of thermal expansion

1.75E-5 - 1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.75E-5 - 1.8E-5 1/K at 23.0 °C

23.0 °C

Melting point

870 °C

Show Material materials with Melting point of 870 °C

Specific heat capacity

360 J/(kg·K)

Show Material materials with Specific heat capacity of 360 J/(kg·K) at 23.0 °C

23.0 °C

Thermal conductivity

105 - 110 W/(m·K)

Show Material materials with Thermal conductivity of 105 - 110 W/(m·K) at 23.0 °C

23.0 °C

Electrical

PropertyValueTemperature

Electrical resistivity

6.2E-6 - 7.8E-6 Ω·m

Show Material materials with Electrical resistivity of 6.2E-6 - 7.8E-6 Ω·m at 23.0 °C

23.0 °C

Specific Electrical conductivity

22 - 28 % IACS

Show Material materials with Specific Electrical conductivity of 22 - 28 % IACS

Chemical properties

Property

Aluminium

0 - 0.2 %

Beryllium

1.8 - 2 %

Cobalt

0.2 %

min. Nickel + Cobalt

Copper

96.1 - 98 %

Balance

Iron

0 - 0.6 %

max., Nickel + Cobalt + Iron

Nickel

0.2 - 0.6 %

min. Nickel + Cobalt

Other

0 - 0.5 %

Silicon

0 - 0.2 %

Technological properties

Property
Application areas

Typical applications include precision coil springs and pins for burn-in and test socket contacts and probe pins, computer processor socket contacts, cold headed fasteners, modular jack contacts, woven mesh electromagnetic shielding gaskets and resilient eyeglass frames.