See where ASTM Grade 23 Annealed falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ4.4 g/cm³ at 23 °C
Coefficient of thermal expansion
α9.4E-6 1/K at 23 °C
Melting point
Tm1500 - 1750 °C
Typical for Titanium Alpha Beta Alloy
Specific heat capacity
cp560 J/(kg·K) at 23 °C
Thermal conductivity
λ7.1 W/(m·K) at 23 °C
Element
Weight %
Comment
88.1 - 91 %
5.5 - 6.5 %
3.5 - 4.5 %
0 - 0.08 %
0 - 0.01 %
This material data has been provided by MakeItFrom.com.