Density
ρ8.9 g/cm³ at 23 °C
Coefficient of thermal expansion
α1.3E-5 1/K at 23 °C
Melting point
Tm1440 °C
Specific heat capacity
cp460 J/(kg·K) at 23 °C
Thermal conductivity
λ70 W/(m·K) at 23 °C
Element
Weight %
Comment
99 - 100 %
0 - 0.15 %
0 - 0.25 %
0 - 0.4 %
0 - 0.35 %