General
Property | Value | Temperature |
---|---|---|
Density | 8.4 g/cm³ Show Material materials with Density of 8.4 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature |
---|---|---|
Elastic modulus | 230 GPa Show Material materials with Elastic modulus of 230 GPa at 23.0 °C | 23.0 °C |
Elongation | 75 % Show Material materials with Elongation of 75 % at 23.0 °C | 23.0 °C |
Tensile strength | 980 MPa Show Material materials with Tensile strength of 980 MPa at 23.0 °C | 23.0 °C |
Yield strength | 520 MPa Show Material materials with Yield strength of 520 MPa at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature |
---|---|---|
Coefficient of thermal expansion | 1.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K at 23.0 °C | 23.0 °C |
Specific heat capacity | 430 J/(kg·K) Show Material materials with Specific heat capacity of 430 J/(kg·K) at 23.0 °C | 23.0 °C |
Chemical properties
Property | ||
---|---|---|
Boron | 0 - 1E-3 % | |
Carbon | 0 - 0.15 % | |
Chromium | 18.5 - 21.5 % | |
Cobalt | 39 - 42 % | |
Iron | 7.6 - 20 % | |
Manganese | 1 - 2 % | |
Molybdenum | 6.5 - 7.5 % | |
Nickel | 15 - 18 % | |
Phosphorus | 0 - 0.02 % | |
Silicon | 0 - 1.2 % | |
Sulfur | 0 - 0.015 % |