General

Density

ρ

8.7 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

230 GPa at 23 °C

Show Unclassified Cobalt Alloy materials with Elastic modulus of 230 GPa at 23 °C

Elongation

A

47 % at 23 °C

Show Unclassified Cobalt Alloy materials with Elongation of 47 % at 23 °C

Tensile strength

Rm

770 MPa at 23 °C

Show Unclassified Cobalt Alloy materials with Tensile strength of 770 MPa at 23 °C

Yield strength

YS

310 MPa at 23 °C

Show Unclassified Cobalt Alloy materials with Yield strength of 310 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

1.3E-5 1/K at 23 °C

Melting point

Tm

1320 °C

Specific heat capacity

cp

500 J/(kg·K) at 23 °C

Thermal conductivity

λ

11 W/(m·K) at 23 °C

Chemical properties

Element

Weight %

Comment

Ni

33 - 37 %

Co

29.1 - 39 %

Cr

19 - 21 %

Mo

9 - 10.5 %

B

0 - 0.015 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.