See where UNS R30008 Cold Worked And Aged falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ8.4 g/cm³ at 23 °C
Coefficient of thermal expansion
α1.3E-5 1/K at 23 °C
Specific heat capacity
cp430 J/(kg·K) at 23 °C
Element
Weight %
Comment
39 - 42 %
18.5 - 21.5 %
15 - 18 %
7.6 - 20 %
6.5 - 7.5 %
This material data has been provided by MakeItFrom.com.