Nickel 200 Cold Worked

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.9 g/cm³

Show Material materials with Density of 8.9 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

210 GPa

Show Material materials with Elastic modulus of 210 GPa

Elongation

23.0 °C

23 %

Show Material materials with Elongation of 23 %

Tensile strength

23.0 °C

550 MPa

Show Material materials with Tensile strength of 550 MPa

Yield strength

23.0 °C

370 MPa

Show Material materials with Yield strength of 370 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.3E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.3E-5 1/K

Melting point

1440 °C

Show Material materials with Melting point of 1440 °C

Specific heat capacity

23.0 °C

460 J/(kg·K)

Show Material materials with Specific heat capacity of 460 J/(kg·K)

Thermal conductivity

23.0 °C

70 W/(m·K)

Show Material materials with Thermal conductivity of 70 W/(m·K)

Chemical properties

PropertyValue

Carbon

0 - 0.15 %

Show Material materials with Carbon of 0 - 0.15 %

Copper

0 - 0.25 %

Show Material materials with Copper of 0 - 0.25 %

Iron

0 - 0.4 %

Show Material materials with Iron of 0 - 0.4 %

Manganese

0 - 0.35 %

Show Material materials with Manganese of 0 - 0.35 %

Nickel

99 - 100 %

Show Material materials with Nickel of 99 - 100 %

Silicon

0 - 0.35 %

Show Material materials with Silicon of 0 - 0.35 %

Sulfur

0 - 0.01 %

Show Material materials with Sulfur of 0 - 0.01 %