UNS R30605 Cold Worked

Want to keep this datasheet? Save it now in your required format

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

10 g/cm³

Show Material materials with Density of 10 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

210 GPa

Show Material materials with Elastic modulus of 210 GPa

Elongation

23.0 °C

35 %

Show Material materials with Elongation of 35 %

Tensile strength

23.0 °C

1900 MPa

Show Material materials with Tensile strength of 1900 MPa

Yield strength

23.0 °C

1600 MPa

Show Material materials with Yield strength of 1600 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.2E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.2E-5 1/K

Melting point

1330 °C

Show Material materials with Melting point of 1330 °C

Specific heat capacity

23.0 °C

390 J/(kg·K)

Show Material materials with Specific heat capacity of 390 J/(kg·K)

Thermal conductivity

23.0 °C

9.4 W/(m·K)

Show Material materials with Thermal conductivity of 9.4 W/(m·K)

Chemical properties

PropertyValue

Carbon

0.05 - 0.15 %

Show Material materials with Carbon of 0.05 - 0.15 %

Chromium

19 - 21 %

Show Material materials with Chromium of 19 - 21 %

Cobalt

46.4 - 57 %

Show Material materials with Cobalt of 46.4 - 57 %

Iron

0 - 3 %

Show Material materials with Iron of 0 - 3 %

Manganese

1 - 2 %

Show Material materials with Manganese of 1 - 2 %

Nickel

9 - 11 %

Show Material materials with Nickel of 9 - 11 %

Phosphorus

0 - 0.04 %

Show Material materials with Phosphorus of 0 - 0.04 %

Silicon

0 - 0.4 %

Show Material materials with Silicon of 0 - 0.4 %

Sulfur

0 - 0.03 %

Show Material materials with Sulfur of 0 - 0.03 %

Tungsten

14 - 16 %

Show Material materials with Tungsten of 14 - 16 %