UNS C10700 H01

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

9 g/cm³

Show Material materials with Density of 9 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

120 GPa

Show Material materials with Elastic modulus of 120 GPa

Poisson's ratio

23.0 °C

0.34 [-]

Show Material materials with Poisson's ratio of 0.34 [-]

Typical for Wrought Copper Pure / Low Alloyed Copper

Shear modulus

23.0 °C

48 GPa

Show Material materials with Shear modulus of 48 GPa

Typical for Wrought Copper Pure / Low Alloyed Copper

Tensile strength

23.0 °C

270 MPa

Show Material materials with Tensile strength of 270 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.6E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.6E-5 1/K

Melting point

1080 °C

Show Material materials with Melting point of 1080 °C

Specific heat capacity

23.0 °C

390 J/(kg·K)

Show Material materials with Specific heat capacity of 390 J/(kg·K)

Thermal conductivity

23.0 °C

390 W/(m·K)

Show Material materials with Thermal conductivity of 390 W/(m·K)

Chemical properties

PropertyValue

Copper

99.83 - 99.92 %

Show Material materials with Copper of 99.83 - 99.92 %

Other

0 - 0.05 %

Show Material materials with Other of 0 - 0.05 %

Oxygen

0 - 1E-3 %

Show Material materials with Oxygen of 0 - 1E-3 %

Silver

0.09 - 0.12 %

Show Material materials with Silver of 0.09 - 0.12 %