UNS C51000 H02

View suppliers (34)
Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.8 g/cm³

Show Material materials with Density of 8.8 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

110 GPa

Show Material materials with Elastic modulus of 110 GPa

Elongation

23.0 °C

28 %

Show Material materials with Elongation of 28 %

Poisson's ratio

23.0 °C

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Leaded Phosphor Bronze

Tensile strength

23.0 °C

460 MPa

Show Material materials with Tensile strength of 460 MPa

Yield strength

23.0 °C

380 MPa

Show Material materials with Yield strength of 380 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K

Melting point

960 °C

Show Material materials with Melting point of 960 °C

Specific heat capacity

23.0 °C

380 J/(kg·K)

Show Material materials with Specific heat capacity of 380 J/(kg·K)

Thermal conductivity

23.0 °C

77 W/(m·K)

Show Material materials with Thermal conductivity of 77 W/(m·K)

Chemical properties

PropertyValue

Copper

92.9 - 95.5 %

Show Material materials with Copper of 92.9 - 95.5 %

Iron

0 - 0.1 %

Show Material materials with Iron of 0 - 0.1 %

Lead

0 - 0.05 %

Show Material materials with Lead of 0 - 0.05 %

Other

0 - 0.5 %

Show Material materials with Other of 0 - 0.5 %

Phosphorus

0.03 - 0.35 %

Show Material materials with Phosphorus of 0.03 - 0.35 %

Tin

4.5 - 5.8 %

Show Material materials with Tin of 4.5 - 5.8 %

Zinc

0 - 0.3 %

Show Material materials with Zinc of 0 - 0.3 %

Looking for suppliers of this material? Click to see 34 supplier of UNS C51000 H02 on Matmatch