UNS C52100 H02

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueTemperature

Density

8.8 g/cm³

Show Material materials with Density of 8.8 g/cm³ at 23.0 °C

23.0 °C

Mechanical

PropertyValueTemperatureComment

Elastic modulus

110 GPa

Show Material materials with Elastic modulus of 110 GPa at 23.0 °C

23.0 °C

Elongation

32 %

Show Material materials with Elongation of 32 % at 23.0 °C

23.0 °C

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-] at 23.0 °C

23.0 °C

Typical for Leaded Phosphor Bronze

Tensile strength

530 MPa

Show Material materials with Tensile strength of 530 MPa at 23.0 °C

23.0 °C

Yield strength

380 MPa

Show Material materials with Yield strength of 380 MPa at 23.0 °C

23.0 °C

Thermal

PropertyValueTemperature

Coefficient of thermal expansion

1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K at 23.0 °C

23.0 °C

Melting point

880 °C

Show Material materials with Melting point of 880 °C

Specific heat capacity

380 J/(kg·K)

Show Material materials with Specific heat capacity of 380 J/(kg·K) at 23.0 °C

23.0 °C

Thermal conductivity

62 W/(m·K)

Show Material materials with Thermal conductivity of 62 W/(m·K) at 23.0 °C

23.0 °C

Chemical properties

Property

Copper

89.8 - 93 %

Iron

0 - 0.1 %

Lead

0 - 0.05 %

Other

0 - 0.5 %

Phosphorus

0.03 - 0.35 %

Tin

7 - 9 %

Zinc

0 - 0.2 %