General

Density

ρ

9 g/cm³ at 20 °C

Mechanical

Elastic modulus

E

120 GPa at 20 °C

Show Wrought Copper Pure / Low Alloyed Copper materials with Elastic modulus of 120 GPa at 20 °C

Tensile strength

Rm

320 MPa at 20 °C

Show Wrought Copper Pure / Low Alloyed Copper materials with Tensile strength of 320 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

1.6E-5 1/K at 20 °C

Melting point

Tm

1080 °C

Specific heat capacity

cp

390 J/(kg·K) at 20 °C

Thermal conductivity

λ

390 W/(m·K) at 20 °C

Electrical

Electrical conductivity

σel

5.80E+8 S/m at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

99.95 - 100 %

O

0 - 1E-3 %

This material data has been provided by MakeItFrom.com.