General
Property | Value | Temperature |
---|---|---|
Density | 9 g/cm³ Show Material materials with Density of 9 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 120 GPa Show Material materials with Elastic modulus of 120 GPa at 23.0 °C | 23.0 °C | |
Elongation | 20 % Show Material materials with Elongation of 20 % at 23.0 °C | 23.0 °C | |
Poisson's ratio | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] at 23.0 °C | 23.0 °C | Typical for Wrought Copper Pure / Low Alloyed Copper |
Shear modulus | 48 GPa Show Material materials with Shear modulus of 48 GPa at 23.0 °C | 23.0 °C | Typical for Wrought Copper Pure / Low Alloyed Copper |
Tensile strength | 320 MPa Show Material materials with Tensile strength of 320 MPa at 23.0 °C | 23.0 °C | |
Yield strength | 280 MPa Show Material materials with Yield strength of 280 MPa at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature |
---|---|---|
Coefficient of thermal expansion | 1.7E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.7E-5 1/K at 23.0 °C | 23.0 °C |
Melting point | 1080 °C Show Material materials with Melting point of 1080 °C | |
Specific heat capacity | 390 J/(kg·K) Show Material materials with Specific heat capacity of 390 J/(kg·K) at 23.0 °C | 23.0 °C |
Thermal conductivity | 390 W/(m·K) Show Material materials with Thermal conductivity of 390 W/(m·K) at 23.0 °C | 23.0 °C |
Chemical properties
Property | ||
---|---|---|
Copper | 99.99 - 100 % | |
Lead | 0 - 1E-3 % | |
Oxygen | 0 - 5E-4 % | |
Phosphorus | 0 - 3E-4 % | |
Zinc | 0 - 1E-4 % |