See where UNS C19010 H04 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ8.9 g/cm³ at 20 °C
Coefficient of thermal expansion
α1.6E-5 1/K at 20 °C
Specific heat capacity
cp390 J/(kg·K) at 20 °C
Thermal conductivity
λ260 W/(m·K) at 20 °C
Electrical conductivity
σel2.90E+8 S/m at 20 °C
Element
Weight %
Comment
97.3 - 99.04 %
0.8 - 1.8 %
0.15 - 0.35 %
0.01 - 0.05 %
0 - 0.5 %
This material data has been provided by MakeItFrom.com.