General
Property | Value | Temperature |
---|---|---|
Density | 8.6 g/cm³ Show Material materials with Density of 8.6 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 110 GPa Show Material materials with Elastic modulus of 110 GPa at 23.0 °C | 23.0 °C | |
Elongation | 7 % Show Material materials with Elongation of 7 % at 23.0 °C | 23.0 °C | |
Shear modulus | 40 GPa Show Material materials with Shear modulus of 40 GPa at 23.0 °C | 23.0 °C | Typical for Wrought Copper Brass |
Tensile strength | 500 MPa Show Material materials with Tensile strength of 500 MPa at 23.0 °C | 23.0 °C | |
Yield strength | 410 MPa Show Material materials with Yield strength of 410 MPa at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature |
---|---|---|
Coefficient of thermal expansion | 1.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.9E-5 1/K at 23.0 °C | 23.0 °C |
Melting point | 970 °C Show Material materials with Melting point of 970 °C | |
Specific heat capacity | 380 J/(kg·K) Show Material materials with Specific heat capacity of 380 J/(kg·K) at 23.0 °C | 23.0 °C |
Thermal conductivity | 140 W/(m·K) Show Material materials with Thermal conductivity of 140 W/(m·K) at 23.0 °C | 23.0 °C |
Chemical properties
Property | ||
---|---|---|
Copper | 78.5 - 81.5 % | |
Iron | 0 - 0.05 % | |
Lead | 0 - 0.05 % | |
Other | 0 - 0.2 % | |
Zinc | 18.2 - 21.5 % |