UNS C36000 H04

Want to keep this datasheet? Save it now in your required format

Description

Equivalent Materials

Ashby charts

See where UNS C36000 H04 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

8.4 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

97 GPa at 23 °C

Show Leaded Brass materials with Elastic modulus of 97 GPa at 23 °C

Elongation

A

5.8 % at 23 °C

Show Leaded Brass materials with Elongation of 5.8 % at 23 °C

Shear modulus

G

40 GPa at 23 °C

Show Leaded Brass materials with Shear modulus of 40 GPa at 23 °C

Typical for Wrought Copper Brass

Tensile strength

Rm

540 MPa at 23 °C

Show Leaded Brass materials with Tensile strength of 540 MPa at 23 °C

Yield strength

YS

270 MPa at 23 °C

Show Leaded Brass materials with Yield strength of 270 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

2.1E-5 1/K at 23 °C

Melting point

Tm

890 °C

Specific heat capacity

cp

380 J/(kg·K) at 23 °C

Thermal conductivity

λ

120 W/(m·K) at 23 °C

Chemical properties

Element

Weight %

Comment

Cu

60 - 63 %

Zn

32.5 - 37.5 %

Pb

2.5 - 3.7 %

Fe

0 - 0.35 %

Other

0 - 0.5 %

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.