UNS C65100 H04

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.8 g/cm³

Show Material materials with Density of 8.8 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

120 GPa

Show Material materials with Elastic modulus of 120 GPa

Elongation

23.0 °C

12 %

Show Material materials with Elongation of 12 %

Poisson's ratio

23.0 °C

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Leaded Phosphor Bronze

Tensile strength

23.0 °C

480 MPa

Show Material materials with Tensile strength of 480 MPa

Yield strength

23.0 °C

330 MPa

Show Material materials with Yield strength of 330 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K

Melting point

1030 °C

Show Material materials with Melting point of 1030 °C

Specific heat capacity

23.0 °C

380 J/(kg·K)

Show Material materials with Specific heat capacity of 380 J/(kg·K)

Thermal conductivity

23.0 °C

57 W/(m·K)

Show Material materials with Thermal conductivity of 57 W/(m·K)

Chemical properties

PropertyValue

Copper

94.5 - 99.2 %

Show Material materials with Copper of 94.5 - 99.2 %

Iron

0 - 0.8 %

Show Material materials with Iron of 0 - 0.8 %

Lead

0 - 0.05 %

Show Material materials with Lead of 0 - 0.05 %

Manganese

0 - 0.7 %

Show Material materials with Manganese of 0 - 0.7 %

Other

0 - 0.5 %

Show Material materials with Other of 0 - 0.5 %

Silicon

0.8 - 2 %

Show Material materials with Silicon of 0.8 - 2 %

Zinc

0 - 1.5 %

Show Material materials with Zinc of 0 - 1.5 %