See where UNS C75700 H04 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ8.5 g/cm³ at 23 °C
Coefficient of thermal expansion
α1.6E-5 1/K at 23 °C
Melting point
Tm875 - 1135 °C
Typical for Wrought Copper Nickel Silver Grade
Specific heat capacity
cp390 J/(kg·K) at 23 °C
Thermal conductivity
λ40 W/(m·K) at 23 °C
Element
Weight %
Comment
63.5 - 66.5 %
19.2 - 25.5 %
11 - 13 %
0 - 0.25 %
0 - 0.05 %
This material data has been provided by MakeItFrom.com.