General
Property | Value | Temperature |
---|---|---|
Density | 8.9 g/cm³ Show Material materials with Density of 8.9 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Thermal
Property | Value | Temperature | Comment |
---|---|---|---|
Coefficient of thermal expansion | 1.6E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.6E-5 1/K at 23.0 °C | 23.0 °C | |
Melting point | 855 - 1090 °C Show Material materials with Melting point of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Specific heat capacity | 390 J/(kg·K) Show Material materials with Specific heat capacity of 390 J/(kg·K) at 23.0 °C | 23.0 °C | |
Thermal conductivity | 260 W/(m·K) Show Material materials with Thermal conductivity of 260 W/(m·K) at 23.0 °C | 23.0 °C |
Chemical properties
Property | ||
---|---|---|
Copper | 97.3 - 99.04 % | |
Nickel | 0.8 - 1.8 % | |
Other | 0 - 0.5 % | |
Phosphorus | 0.01 - 0.05 % | |
Silicon | 0.15 - 0.35 % |