See where UNS C35300 H06 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ8.3 g/cm³ at 20 °C
Coefficient of thermal expansion
α2E-5 1/K at 20 °C
Melting point
Tm890 °C
Specific heat capacity
cp380 J/(kg·K) at 20 °C
Thermal conductivity
λ120 W/(m·K) at 20 °C
Electrical conductivity
σel1.51E+8 S/m at 20 °C
Element
Weight %
Comment
60 - 63 %
33.9 - 38.5 %
1.5 - 2.5 %
0 - 0.1 %
0 - 0.5 %
This material data has been provided by MakeItFrom.com.