General
Property | Value | Temperature |
---|---|---|
Density | 8.9 g/cm³ Show Material materials with Density of 8.9 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Thermal
Property | Value | Temperature |
---|---|---|
Coefficient of thermal expansion | 1.5E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.5E-5 1/K at 23.0 °C | 23.0 °C |
Melting point | 1150 °C Show Material materials with Melting point of 1150 °C | |
Specific heat capacity | 400 J/(kg·K) Show Material materials with Specific heat capacity of 400 J/(kg·K) at 23.0 °C | 23.0 °C |
Thermal conductivity | 43 W/(m·K) Show Material materials with Thermal conductivity of 43 W/(m·K) at 23.0 °C | 23.0 °C |
Chemical properties
Property | ||
---|---|---|
Copper | 73.5 - 80.5 % | |
Iron | 0.5 - 1 % | |
Lead | 0 - 0.05 % | |
Manganese | 0 - 1 % | |
Nickel | 19 - 23 % | |
Other | 0 - 0.5 % | |
Zinc | 0 - 1 % |